I don't see where your original question was answered.
Yes, map gas is more than sufficient to that task. Better than just propane but not quite as good a pure acetylene.
I would use a solid 60/40 or 63/37 tin/lead solder (without internal rosin flux.)
This is the type used by stained glass artisans. You can get it a hobby lobby !
arw01 wrote:Wifey wants a peacock made up, since shipping to buy it would be quite high thought I would try making it.How is copper to braze/solder with a map gas torch?
Alan